Paste, Graphite, Heatpipes, or Vapor Chambers? How Mechanical Engineers Can Manage Heat

Image
Pulse
David Bortolami
David Bortolami
Nov 24, 2026

Pick up an ultrabook halfway through a 4K export or a batch of local inference. The aluminum underside is lukewarm, a tiny blower whispers at several thousand RPM, and somewhere inside, a postage-stamp-sized sliver of silicon is dumping 36 watts into a chassis barely twelve millimeters thick.

And yet that heat escapes an enclosure thin enough to slide into the yellow manila envelope Steve Jobs famously emptied on stage in 2008, all while the aluminum chassis stays comfortable to the touch.

Ask an electronic engineer about heat and they will talk primarily about efficiency: conduction losses in copper, gate-drive and switching losses in a MOSFET, and hysteresis in an inductor core. An EE’s primary instinct is prevention: tuning topologies and choosing components so less heat is generated in the first place.

But thermodynamics always takes its toll. Once electrical energy turns into thermal energy, circuit design gives way to thermal and mechanical engineering. If you are reading this, it might be your turn.

In mechanical engineering circles, thermal management is mostly explained as a set of steady-state problems. You might learn how heat diffuses smoothly along a copper pipe, or how to calculate a surface temperature under a constant thermal load and steady-state conditions. You’re far less likely to learn about modern thermal interface materials, or about the dynamic, pulsed and unpredictable heat sources found in modern electronics.

This article aims to fill that gap: an introduction to advanced thermal engineering for electronic devices.

Key Takeaways

  • Comfort and expectations often set the real limit. Long before safety standards kick in, users will complain and perceive the product as not working correctly.
  • Almost every mechanical interface needs a thermal interface material. Machined surfaces are never perfect, and the gaps they leave must be filled with paste, pads or other solutions.
  • Advanced materials are worth a look. Consider pyrolytic graphite sheets and vapor chambers for your next project.
  • Heatpipes trade lift for flow. Finer wick pores hold liquid against gravity but choke its return, so choose the wick for the orientations your product will see.
  • Thermal parts are standard parts too. Keep track of them like any other line in your BOM.

Planning

Before choosing any heat sink, fan, heatpipe or thermal interface material, you must answer three fundamental questions about your system. Together, they should sufficiently constrain the problem:

  • Where does the heat originate?
  • Where does the heat end up?
  • What can we get away with in between?

The Heat Source

The heat source is perhaps the most important component in the whole thermal path.

Apple learned this the hard way. In 2016 it introduced a thinner MacBook Pro, and in July 2018 it fitted the 15-inch model with Intel’s six-core Core i9-8950HK, rated at 45 W and boosting to 4.8 GHz. Under a long video export, the chip could not even hold its 2.9 GHz base clock, and in a benchmark loop it hit its 100 °C limit, making the system extremely sluggish. Apple blamed a firmware bug and patched it within a week, but even afterwards Notebookcheck measured the chip drawing about 90 W at first, then settling at 47–52 W, about all the cooling could handle. In a sustained benchmark the i9 ended up slower than the cheaper i7. The 16-inch model that replaced it in 2019 got a 35% larger heat sink.

Heat sources behave wildly differently. Industrial systems often have constant or slowly cycling loads, which are at least somewhat predictable and can usually be modeled. Computers and smartphones produce short bursts of heat whenever the workload changes unpredictably, for example when the user opens an app or plugs in the charger.

To design an effective system, you need to understand a few fundamental things about the source.

How Much Heat Does Your Source Produce?

Identify the dissipated power both in the worst-case scenario and in an average situation, and consider the losses throughout the entire system. A small industrial power supply that draws 100 W at 90% efficiency, for example, dissipates 10 W as heat.

How Much Surface Area Does Your Source Have?

What matters, engineering-wise, is the heat flux, the power per unit area. The die of a modern laptop processor might measure about 18 × 12 mm (0.71 × 0.47 in), or 2.16 cm² (0.33 in²). If it dissipates 36 W, its heat flux is:

Our 10 W power supply, by contrast, spreads its heat over a board of about 100 × 200 mm (3.9 × 7.9 in), or 200 cm² (31 in²):

Those two numbers differ by a factor of over 300, which can be hard to fathom.

A great way to picture them is to scale them up to the desk in front of you. A standard desk is about 70 cm by 1.4 m (28 × 55 in). Heat it at the same density as the power supply, and it gives off 490 W, about half the midsummer noon sun in Sacramento, California. Apply the density of a modern laptop processor instead, and it gives off 163 kW, more than 160 times the midsummer noon sun.

The high peak flux means that the first few millimeters of the heat path are the most critical. Close to a processor die, the heat has to be removed immediately and as efficiently as possible. That’s why gaming PC builders obsess over the quality of their thermal paste.

How Does the Source Behave Over Time?

This is the question that often gets skipped, and yet it is what separates a mediocre, unreliable product from a great one. Some equipment produces heat at a fairly steady rate for long periods. Industrial electronics are a good example: there may be room for a substantial heat sink, and the brief may favour reliability, low cost and simple construction over minimum size and mass. The job is to move heat away continuously and keep temperatures in a comfortable range.

Other equipment sees an uneven load. The laptop from the introduction spends long stretches at low power, then produces a burst of heat when a render or a local AI model starts. The design must keep the temperature rise in check quickly enough to preserve performance. If the processor reaches its thermal limit, it throttles: it reduces its operating frequency, and the device feels sluggish.

Thermal profiles over time: continuous industrial load versus bursty processor load Continuous versus pulsed thermal loads. Top: a steady industrial load over hours. Bottom: an ultrabook processor idling near 5 W, with bursts up to 64 W. Illustrative, not measured data. 

How Hot Can Your Source Run?

Every chip has a maximum junction temperature (Tj,max), the hottest its transistors are allowed to get: 100 °C for the i9 above, and often 125–175 °C for other chips and power transistors. Beyond it, the maker no longer guarantees that the part will work, or for how long. But long before a chip shuts down, heat slowly undermines its reliability. Heat makes atoms jiggle, and with enough jiggling some of them move for good. In the thin copper wires on a chip, the flowing electrons push the metal atoms along, a process called electromigration, which slowly opens voids in some places and piles up metal in others, until a line breaks or shorts to its neighbor. In the solder joints between a PCB and its components, brittle intermetallic layers grow at the interface, and every heat-up and cool-down cycle spreads cracks through the joint.

Something to be aware of: the thermal behavior of a part can change during its life cycle, even though its electrical parameters stay the same. China’s packaging industry has grown enormously in the past few years, and it had nearly 200 assembly and test plants, and in 2024 mainland China hosted about 28% of the world’s chip assembly, packaging and test capacity. Many chip makers now package and test their parts there, including Intel and Onsemi, and while packaging changes generally do not affect a part electrically, they can radically change its thermal properties. These changes are often announced in product change notices, but they are easy to miss, so always check the manufacturer’s current datasheet, for example from the part’s page on Octopart.

Many of these mechanisms follow the Arrhenius law: as a rule of thumb, for a typical activation energy of about 0.7 eV, every sustained 10 K rise in junction temperature roughly doubles their failure rate. Fatigue cracks in solder are the exception; they depend on how often, and by how much, the temperature swings.

Does Your Source Support Active Throttling, and What Is the Trade-off?

Throttling, i.e. dynamically reducing the thermal load when temperatures get too high, can serve as an emergency safety net or as the core operating strategy of your product’s thermal management. In modern laptops and smartphones, processors are deliberately allowed to draw well above their continuous cooling budget, called thermal design power (TDP), for seconds to tens of seconds (Intel recommends averaging over about 28 seconds), burning through their thermal reserves to deliver snappy responses, then dialling back before the chassis overheats.

The difficult part is that throttling is an interaction design problem and a user experience problem as much as a thermal one. On your phone, a sudden clock-speed reduction that drops video frames during playback or causes audio stutter makes the device seem faulty, whereas the same slowdown during a three-hour background task goes unnoticed. Designing for throttling requires deciding what degree of performance determinism your user expects, keeping in mind that user experience can often be traded off against reliability, through the aforementioned Arrhenius relationship.

Where the Heat Ends Up

  • Surface area and airflow. Sealed enclosures protect internal components from dust and water ingress and offer high long-term reliability, but their ability to shed heat depends entirely on surface area, enclosure orientation and natural convection. Forced convection with blowers or fans dramatically increases the amount of heat dissipated, but at the cost of noise, dust and fan reliability.
  • Environment. Thermal headroom is always relative to ambient temperature. A device left behind the windscreen of a car on a sunny summer afternoon can reach 60 °C before it is even powered on: measured cabin temperatures in parked cars run from 41 to 76 °C. The same applies to industrial electronics inside a non-ventilated cabinet.
  • User expectation. A mechanic putting their hand on an industrial motor drive expects it to be hot. A gamer picking up a gamepad expects it to stay cool; if it reaches 45 °C, they assume the battery is failing. If your product runs hotter than users expect, you might be in for a world of pain, and a lot of customer service calls.

Touch Temperature Limits

Two of the most popular safety standards used in the industry for surface touch temperatures are IEC 62368-1, for consumer and IT equipment, and IEC 60601-1, for medical devices. Both set their limits based on the material of the surface and the amount of time the user can be expected to touch it.

For medical electrical equipment, IEC 60601-1 sets the following limits:

Contact time

Metal

Glass/ceramic

Plastic/wood

Under 1 s

74 °C

80 °C

86 °C

1–10 s

56 °C

66 °C

71 °C

10 s – 1 min

51 °C

56 °C

60 °C

1 min or more

48 °C

48 °C

48 °C

Consumer and IT equipment falls under IEC 62368-1, which uses a similar scheme:

Contact time

Metal

Glass/ceramic

Plastic

Under 1 s

70 °C

80 °C

94 °C

1–10 s

60 °C

71 °C

77 °C

10 s – 1 min

51 °C

56 °C

60 °C

1 min – 8 h

48 °C

48 °C

48 °C

Over 8 h, worn on the body

43–48 °C

43–48 °C

43–48 °C

While regulations are useful to guarantee that your product won’t harm your users, they won’t save you from user complaints. Temperatures well below the safety limits may still feel uncomfortable, and translating the subjective perception of heat into an objective, replicable engineering requirement is notoriously difficult. However, human perception studies have provided some useful ranges:

  • Warm (33–35 °C): Skin begins to register warmth above its resting baseline.
  • Comfortable (36–38 °C): In Cornell tests with a tablet-size heated surface, 38 °C felt warm but still comfortable, while 42 °C felt hot and slightly uncomfortable.
  • Uncomfortable (39–42 °C): In a smartphone gaming trial, 75% of participants reported discomfort after 20 minutes on phones whose surfaces settled at about 39 °C and 44 °C.
  • Painful (42–45 °C): Cutaneous nociceptors activate heat-pain signaling at an average threshold of 42–44 °C depending on anatomical location.

Heat Transfer Materials

Copper and Aluminum

Both aluminum and copper are excellent at conducting and spreading heat, but by any measure, neither of them is that impressive at storing it.

Material

cp (J/(kg·K))

Density (kg/m³)

Volumetric heat capacity (MJ/(m³·K))

Aluminum

900

2,700

2.4

Copper

387

8,920

3.5

Water

4,186

1,000

4.2

The specific heat capacity (cp) indicates how much energy a kilogram of material can absorb per kelvin of temperature rise. A kilogram of water stores about 4.7 times as much heat as aluminum and 10.8 times as much as copper.

Heat capacity is one of the fundamental reasons life on Earth is so comfortable. Oceans cover 70% of the planet, and their top 3 m (10 ft) alone store more heat than the entire atmosphere, so they soak up the summer and give it back in winter.

The most important parameter for a physical part is the total heat capacity, in J/K, which you can get by multiplying the specific heat capacity by the mass:

For example, a 50 g aluminum spreader holds about 45 J per kelvin. Heated with a steady 15 W from room temperature, it will take only 54 seconds to become hot to the touch (from 25 °C to 43 °C).

Graphite Sheet

Pyrolytic graphite sheet (PGS) is a thin film of highly oriented graphite, often used to spread heat across a phone or laptop chassis. PGS’s conductivity depends strongly on the orientation of the graphite layers. In the X–Y plane, it can conduct nearly five times better than copper (up to 1,950 W/(m·K)); through its thickness (Z) it is a poor conductor, as low as 3.4 W/(m·K). This incredible property is called orthotropic thermal conductivity, and it makes PGS brilliant at taking a concentrated hot spot and spreading it across a larger area.

When selecting pyrolytic graphite, you should make sure to check the datasheet for exact grades and constructions. Some products are bare graphite. Others are laminated with PET or polyimide film and adhesive. Panasonic alone sells PGS under dozens of EYG-S part numbers, one per size, thickness and laminate; searching the prefix on Octopart lists them all, with datasheets.

Product

Country

Thickness

In-plane (W/(m·K))

Through-plane (W/(m·K))

Stated method

Panasonic PGS

Japan

10–100 µm

700–1,950

Not stated

Not stated

NeoGraf eGRAF SPREADERSHIELD

US

17–50 µm

1,350–1,600

3.4

In-house; ASTM D5470 modified

Jones Tech 6-70-0017-PA

China

17 µm

≥1,500

5–10

Thermal wave

t-Global T68

Taiwan

25 µm

1,500

5

Angstrom; ASTM D5470-06

FRD GR 1500-025

China

25 µm

1,500

15

Laser flash, both axes

Guangdong SQ SQ-H1025

China

22–27 µm

1,350–1,650

8

XY: ASTM E1461; Z: ASTM D5470

Jiangxi Dasen DSN5025

China

25 µm

1,500–1,700

10–15

Not stated

Thermal Interface Materials

The most common family of thermal interface materials consists of a silicone matrix loaded with thermally conductive particles, usually ceramics such as alumina or boron nitride. Depending on the viscosity, the result is either a thermal paste or a thermal pad. Think of it like mayonnaise, an emulsion: the particles are separated by the matrix, and just like mayonnaise, if it’s poorly made, it can separate.

Anyone doing thermal engineering has at some point asked themselves: are TIMs really needed? They’re sometimes gross, goopy, and just another line in the BOM that requires you to draft a standard operating procedure (SOP) on how to apply them.

The answer is yes: thermal interface materials are almost always necessary.

Put a straightedge on a freshly machined aluminum plate and it may look flat. But can you feel the texture with the ridges of your fingerprints? And how planar is it really? As any good mechanical engineer knows, flatness is just a measure of how much surface imperfection we are willing to tolerate.

Where heat transfer is concerned, any machined surface is hopelessly imperfect. Two surfaces may offer enough contact area for them to transfer a mechanical force effectively, but at a microscopic level, for heat to be transferred, the atoms have to be close enough to wiggle together.

Thermal interface materials fill the gaps between imperfect surfaces, where only 1–2% of the area actually touches.

Dry contact versus compressed TIM for rough, machined and bowed faces (a) surface roughness, (b) ridges left by a slightly tilted flat end mill on both faces, (c) faces dished away from each other. Left: dry contact. Right: properly compressed TIM. Not to scale.

Thermal Pads

Every component in a thermal pad formulation has a precise role:

  • The filler carries the heat.
  • The silicone lets the material conform and stay put, much like the gluten in a good loaf of bread.
  • The rest of the formulation dictates how the pad handles, compresses and ages. Thermal pads contain many proprietary additives, and sometimes layers of adhesive or a fiberglass core.

Pads are quite straightforward to use and understand, and that’s perhaps why they are so popular. But if there is one common mistake to watch out for, it’s confusing the test methods used to specify a pad’s performance.

The two most common methods are ASTM D5470, which clamps a sample between meter bars, and the hot-disk method (ISO 22007-2), which measures the bulk material with a heated sensor.

ASTM D5470: a sample clamped between two instrumented metal bars, heater above and cold plate below, with the temperature profile through the stack; hot disk: a thin spiral sensor sandwiched between two pieces of sample, with its temperature rise over time (a) ASTM D5470 drives steady heat through a sample and measures the temperature drop across the entire length, including contact resistance. (b) The hot disk heats a thin sensor between two pieces of sample and reads its temperature rise over a few seconds. 

There is no direct way to convert between them, and the gap, pun intended, can be large:

Product

Form

ASTM D5470 (W/(m·K))

Hot disk (W/(m·K))

Fujipoly SARCON XR-m

Pad

17

11

Lipoly T-work9000

Gel pad

20

12

Before comparing two datasheets, check that they use the same method, the same thickness and the same clamping pressure.

Watch the small print too: t-Global, for example, rates its TG-A9000 pads at 9.0 W/(m·K) by a modified ASTM D5470.

Reliability is manufacturer- and formulation-specific as well. Depending on the product, the failure modes to ask about include oil bleed, slumping on vertical surfaces, hardening, and drying out. For demanding applications, get the exact material’s test data and validate it at your actual temperature, pressure, orientation and service life. That data is often proprietary, and might only be available under NDA.

Thermal Paste

Thermal paste, or thermal grease, is ideal for surfaces that already fit closely and whose flatness can be tightly controlled, such as a CPU lid and its cooler, where it squeezes down to a thin layer only a few tens of micrometers thick. The thickness matters: the thinner the layer, the lower the thermal resistance.

Shin-Etsu, the Japanese silicone maker, is a great example, and one of the laptop industry’s worst-kept secrets. One of its most popular pastes, X-23-7921-5, is rated at 6.0 W/(m·K), modest next to the pads discussed earlier, but it squeezes down to a minuscule 25 µm bond line.

The thinness of the bond line is why thermal paste performs so well. The thermal resistance of a layer is its thickness t divided by its conductivity k and its area A:

Take the 18 × 12 mm die from earlier, dissipating 36 W, and two materials with the same 6 W/(m·K) rating: a 0.5 mm pad and a 25 µm layer of paste. The pad comes out at 0.39 K/W, so the die runs about 14 K hotter than the cooler above it. The paste comes out at 0.019 K/W, a drop of just 0.7 K.

Datasheets for even the most basic pastes reflect this. Wakefield’s zinc-oxide 120-SA is rated at only 0.735 W/(m·K), but at 25 µm over a square inch its thermal resistance is just 0.05 K/W.

Liquid Metal and Indium

When even the best thermal paste becomes a bottleneck, metallic interfaces are the last resort. For years they stayed inside high-tech semiconductor packages. Now device manufacturers are adopting them for high-end consumer applications too. ASUS hand-applied liquid metal in its ROG Mothership gaming laptop in 2019, built a patented machine to apply it in 2020, and by 2021 was using it in every ROG laptop. Sony uses it in the PlayStation 5.

They fall into two main categories:

  • Gallium liquid alloys. They wet both surfaces and spread into a very thin layer, so the resulting thermal joint has almost no resistance. However, they conduct electricity, so it’s necessary to design a barrier around them, as Sony patented for the PlayStation 5. As if that weren’t enough, they attack aluminum, turning it so brittle you can crumble it with your bare hands like a slice of dry toast.
  • Soft indium foils. Indium conducts better, at 86 W/(m·K), and cannot spill or corrode anything, but it fills the surface roughness only by deforming. That requires a clamping pressure of about 140–280 kPa (20–40 psi), so any mounting bracket will have to be stiff and the chip package must be strong enough to take the load.

Advanced Heat Transfer Technologies

At some point, many advanced designs using only heat conduction run out of road.

A copper rod 10 mm in diameter carrying 30 W can only be about 105 mm long before one end gets to 125 °C while the other stays at a comfortable 25 °C.

Even natural single-crystal diamond, the best natural bulk thermal conductor, only stretches that to about half a meter.

When you’re thinking of using silver instead of copper, have squeezed the thermal paste down to twenty micrometers, and laid down synthetic graphite to smear out every hot spot, yet your design somehow weighs two kilograms more than it should, it’s a sign you need to change the fundamental physics of how you’re moving the heat around. When solid conduction fails, you have to stop diffusing heat atom-by-atom and start physically transporting it through a moving fluid.

The Latent Heat Engine

The secret behind the way a heatpipe works is water’s astronomical latent heat of vaporisation.

Warming a gram of liquid water by one kelvin absorbs 4.2 joules of heat. Evaporate that same gram of water at 60 °C under partial vacuum, and it swallows 2,360 joules without warming by even a fraction of a degree. To carry 30 W away from a processor die, a heatpipe needs to boil off only 13 milligrams of water per second, or roughly 46 grams an hour.

Stripped of supplier mystique, a heatpipe is essentially a pump with no moving parts. It works in a closed loop.

A heatpipe in section: heat enters the evaporator, vapor flows along the core, condenses at the condenser, and the liquid returns through the wick

The loop runs in four steps:

  1. Evaporation: At the heated end, called the evaporator, thermal energy boils water out of a porous wick lining the inner copper wall.
  2. Vapor transit: The vapor expands into the low-pressure core and rushes towards the cold end. Carrying 30 W in a 6 mm pipe, it moves at about 8 m/s.
  3. Condensation: At the cooled end, called the condenser, the vapor condenses on the wall and gives up its latent heat to the fins.
  4. Capillary return: The wick brings the water back by capillary action.

The trick of using capillary action and surface tension as a motorless pump sat dormant for two decades after Richard Gaugler first patented a wicked tube for General Motors refrigerators in 1942. It took the nuclear space race to bring it to the forefront of engineering. In 1963, George Grover at Los Alamos National Laboratory, designing power reactors for orbital satellites, independently reinvented the device and named it the “heatpipe”; his team built the first prototypes using water and liquid sodium.

By 1968, a heatpipe was controlling temperatures on GEOS-II, a NASA satellite in orbit; in the 1970s, over 100,000 passive thermosiphons, wickless heatpipes that return their liquid by gravity, were installed to keep the permafrost frozen along the Trans-Alaska Pipeline. Yet heatpipes did not become everyday consumer items until the mid-1990s, when scorching Intel Pentium processors arrived in thin laptop chassis.

Choosing the Wick: Suction Versus Drag

The wick dictates how much power the heatpipe can carry and how much tilt it can tolerate.

Two fundamental numbers describe a wick. The first is the effective pore radius, reff: the smaller the pores, the harder the wick pulls. Set that suction against gravity and you get the height to which a wick can lift water:

The second is permeability, K, measured in m², which says how easily liquid seeps through the wick. Pushing a mass flow m of liquid with viscosity  along a wick of length L and cross-section A costs:

Commercially available designs use four main construction methods:

  • Wickless. Also called thermosiphons, wickless heatpipes are essentially smooth tubes with no wick. Liquid returns by gravity alone, so the evaporator must always sit below the condenser. Turn one upside down and heat transfer stops, a characteristic that can sometimes be exploited to make a one-way thermal diode.
  • Axial grooves. Fine channels, for example 0.3 mm deep at a 0.6 mm pitch, are formed directly in the copper wall. Because the channels are quite wide and open, liquid flows through them with very little viscous drag, allowing a surprisingly high mass flow over long lengths. The trade-off, compared with the other wicks, is pore size: broad grooves produce a small amount of capillary suction (lifting water only 8 to 50 mm against gravity).
  • Screen mesh. Fine woven copper wire mesh pressed against the inner wall. Mesh delivers more capillary lift than grooves, and it bends and flattens well.
  • Sintered copper powder. Copper particles fused into a porous metallic sponge along the inner walls of the heatpipe. Sintered wicks achieve the smallest pore radii of any commercial wick, generating enormous suction and lift against gravity. This makes sintered powder the default for lightweight devices that have to work in any orientation.

The physics presents a fundamental trade-off, which is well illustrated in this table from the NASA Heat Pipe Design Handbook:

Wick

Effective pore radius

Permeability (10−10 m2)

Static water lift at zero flow

Axial grooves

0.25–1.5 mm

35–1,250

8–50 mm

100-mesh screen

0.12 mm

1.8

104 mm

200-mesh screen

0.063 mm

0.55

197 mm

Sintered powder

0.01–0.1 mm

0.1–10

125–1,250 mm

Put simply: the smaller the pores, the higher the wick can hold water up against gravity: from a few centimeters for grooves to over a meter for the finest sintered powder. But the same small pores make the wick far less permeable, so the liquid struggles to flow back.

So no wick is necessarily “the best”: suction grows as 1/reff, while permeability shrinks as r2eff.

Capillary suction falls as 1/r while flow through the wick rises as r², so small pores pull hard but let little liquid through Shrinking the pores strengthens the pull but chokes the flow.

How Is a Sintered Wick Made?

Making a sintered wick is less exotic than it may sound. A solid rod, called a mandrel, is inserted into a copper tube. Copper powder is vibrated into the remaining gap, and the assembly is baked at 800–1,000 °C in a hydrogen-rich atmosphere, which keeps the copper free of oxide. That is below copper’s melting point of 1,085 °C, but hot enough that where the grains touch, they grow a small metal neck, and the powder fuses into a rigid sponge that is roughly half empty space. Finally, the mandrel is pulled out, and the tube is evacuated, charged with a measured dose of degassed water and crimped shut.

Five steps of making a sintered wick: insert the mandrel, vibrate in copper powder, bake in a hydrogen furnace, pull out the mandrel, then evacuate, add water and crimp shut Making a sintered copper wick. Not to scale.

If you want to try the different wicks for yourself, Advanced Thermal Solutions (ATS), a popular American manufacturer of standard heatpipes, is a great place to start: you can evaluate the differences on the bench without committing to any tooling costs. ATS even spells the wick out in its part numbers, S for sintered and G for grooved, so you can simply search for the ATS-HP-D6 prefix on Octopart to see the sintered and grooved 6 mm pipes side by side, with distributor stock.

Gravity and Tilt

The wick’s biggest enemy is gravity. When a device sits flat on a desk and its heatpipe lies horizontal, the capillary suction only has to fight fluid friction. But tilt a laptop on its side or hold a phone upside down, and the evaporator may sit higher than the condenser.

Lifting water against gravity imposes a hydrostatic penalty:

Heatpipe orientation: evaporator below, level with and above the condenser. Orientation and liquid return. With the evaporator above the condenser (c), the wick must also lift the liquid by h, so the pipe can carry far less heat.

Take a 150 mm heatpipe with three different wicks. Gravity requires about 960 Pa for every 100 mm the water has to climb, at 60 °C. Here is the effect on each type of wick:

  • Axial grooves within a heatpipe can hold water up only 8–50 mm (see the table above). A tilt somewhere between 3° and 19° stalls the wick, and that is before the friction of the returning liquid is taken into account.
  • Screen mesh can hold water up 104 mm with 100-mesh screen and 197 mm with finer 200-mesh. The former should stall at around 44°. The latter still works with the pipe on end, but gravity will use about three-quarters of the available capillary budget.
  • Sintered powder with 13 µm pores generates about 10 kPa at 60 °C, enough to hold water up about a meter. With the pipe vertical, gravity takes only about 15% of that, leaving 85% to move the liquid.

With the pipe lying flat, where gravity costs nothing, a coarse wick can carry as much heat as a sintered one, or even more, because the liquid flows back so easily. Tilt the pipe against gravity and the fine pores win. That is why sintered powder is the default in laptops and phones, which get used at every angle.

Rated maximum heat load against tilt for 6 mm and 8 mm sintered heatpipes, falling from evaporator below to evaporator above Rated maximum heat load against tilt for standard sintered heatpipes (Celsia). 

Testing Heatpipes

When testing heatpipes, there are a couple of important rules to follow:

  • Test at all angles. Try ramping up the power at the worst orientation. Alternatively, run the product at 120% load and tilt it.
  • Test dynamic burst recovery. When a heat source such as a CPU spikes from 5 W to 50 W during an app launch, the wick can briefly sustain the burst thanks to the latent heat of the water right behind the hot spot. But if that reserve is exhausted, the pipe enters a dangerous state called dryout.

In the dryout state, a heatpipe will need far more time to recover, and the heat has to be reduced enough that the hotspot can refill with fluid through capillary action.

Vapor Chambers

While a heatpipe moves heat along a line, a vapor chamber is effectively a flat, two-dimensional heatpipe.

The physics works just the same, but the wide surface area of the vapor chamber brings some key advantages. While a heatpipe is amazing at moving heat, eventually the heat has to be spread using either a large aluminum block or the graphite sheets we discussed previously. A vapor chamber, however, can also spread the heat over a large surface.

Additionally, the flat shape is particularly convenient for interfacing with silicon dies and other electronic component packages, removing the need for large copper blocks. Vapor chambers also often cope better than heatpipes when the evaporator ends up above the condenser, partly because the liquid has a shorter path back to the hot spot.

Vapor chambers used to be a premium part, found mostly in gaming laptops and graphics cards. They are now cheap enough to go into phones: Apple added one to the iPhone 17 Pro in September 2025, laser-welded into the aluminum frame. Competition from Chinese suppliers has helped. One market report puts the average price of a standard chamber at about $4.50 in 2025.

For a bench test, standard chambers are also easy to buy in single units, such as t-Global’s 56 × 56 × 3 mm TGVC-56-56-3.0-01, though expect a single-unit price well above that average.

Vapor chambers, however, come with some disadvantages. Flat walls resist internal pressure far less well than a tube: Celsia rates unreinforced chambers to about 110 °C before they start to deform, against about 200 °C for an equivalent heatpipe. Vapor chambers also cost more, and they come flat, or at most bent into an L or a U shape.

Suppliers now quote chambers as thin as 0.2–0.25 mm for phones, but as always, the thinner the heatpipe or vapor chamber, the less material and liquid there is behind the evaporator, increasing the risk of dryout.

Conclusions

Thermal engineering can feel a bit like abstract art. There is hardly ever a single right answer, and that leaves an enormous amount of room for creativity. Perhaps it should be called thermal transfer engineering, as it’s all about how you move the heat around, and that can change everything about your product: how it behaves under load, its weight, shape and size, even its looks.

If you are willing to embrace the latest technologies, like synthetic graphite sheets, liquid metal or a properly designed vapor chamber, you can gain a real competitive advantage over teams still bolting CNC-machined aluminum on at the end.

Whichever path you take, a thermal design will likely be made up of a number of standard off-the-shelf parts, such as pads and thermal paste. To make your life as easy as possible, keep track of every thermal component like any other line in your BOM using the Octopart BOM Tool. Part pages also show how many distributors stock each part. A part listed by only one, like the t-Global vapor chamber above, is a single-source risk to check before you design it in.

Frequently Asked Questions

Why does my laptop slow down when it gets hot?

The CPU can draw well above its cooling budget for up to a few tens of seconds, but then it must dial back before the chassis overheats. If it gets too hot, it has no option but to slow down.

How hot can a chip safely run?

Limits vary by chip: the i9 above tops out at 100 °C, and many other parts allow 125 °C or more. However, that doesn’t mean it’s a good idea to keep them at their limit for a long time: every sustained 10 K below it roughly halves the failure rate.

How hot can a product’s surface get before users complain?

The safety limit depends on the material of the surface and on how long people are expected to touch it. For a metal surface users are expected to keep touching, IEC 62368-1 allows up to 48 °C. However, in research, 42 °C already felt hot and slightly uncomfortable.

Do I need a thermal interface material?

Yes, almost always. Even precision-machined surfaces are never perfectly flat, and only 1–2% of the area actually touches and transfers heat between the parts. Paste, pads or other thermal interface materials fill these gaps, ensuring effective heat transfer.

Is thermal paste better than a thermal pad?

It depends. Thermal paste can squeeze incredibly thin, ensuring a minimal temperature drop across it. However, if their performance is good enough, thermal pads are often more convenient to use and install.

Is liquid metal better than thermal paste?

Liquid metal thermal interface materials are incredibly high-performance. However, they need special mechanical features to keep them in place, and they can damage aluminum parts. Metal foil can be a better choice in many applications.

What is the difference between a heatpipe and a vapor chamber?

A vapor chamber is effectively a flat heatpipe. While a heatpipe moves heat along a line, a vapor chamber spreads it over a surface. Vapor chambers are a newer technology but, used correctly, they can solve many challenges that used to require multiple parts.

What is the best heatpipe?

It depends on your application, but in many cases, particularly in consumer electronics, it will probably be a heatpipe with a sintered copper powder wick. However, if your product is installed in a fixed position and needs to dissipate a lot of heat, you might consider grooved heatpipes or even thermosiphons.

Read More Articles